Cooling fin

Deburring at edge face after cutting process

Effects after installation

BEFORE

Tool
Wire brush
Problem
Burrs remained after deburring process because of complicated shape of workpiece.

AFTER

Tool
Effect
No burrs left and finish quality improved.

Workpiece information

Industry
Automotive
Part name
Cooling fin
Material type
Aluminum alloy
Cutting process
Others

Processing conditions

<iframe width="560" height="315" src="https://www.youtube.com/embed/XFuuquxXKvg" frameborder="0" allowfullscreen></iframe>
Tool
Processing detail
Deburring at edge face after cutting process
Rotation speed(min<sup>-1</sup>)
3,000
Feed, feed rate(mm/min)
1,800
Depth of cut (mm)
1.0
Machining time (sec)
-